Weber joint sealants, supplied across the UAE by Lapiz Blue

A movement joint only works if what fills it can move. Weber makes polysulphide and polyurethane sealants for exactly that, in gun grade for vertical joints and pouring grade for horizontal ones. Lapiz Blue supplies them across the UAE. The quantity depends on the joint, not the area, so tell us the joint width, the depth and the total run and we will work back to the number of packs, along with the primer and backer rod the joint needs to perform as designed.

Visit Weber (Saint-Gobain) Official Website
Joint in section: concrete either side, backer rod, primer on the faces, polyurethane or polysulphide sealant
Joint in section: concrete either side, backer rod, primer on the faces, polyurethane or polysulphide sealant

A sealant joint works when the depth is half the width, the backer rod sets that depth, the faces are primed, and the sealant is one that moves. Width is set by the movement, not the gap you were left with.

The range. All 4.

Applications and Best-Fit Scenarios

1

Expansion and movement joints in concrete floors and walls

2

Perimeter joints where a floor meets a wall

3

Horizontal joints in trafficked areas, using the pouring grade

4

Vertical and overhead joints, using the gun grade

How to Choose the Right Sealant

1

Decide the grade by the joint orientation, gun grade for vertical and pouring grade for horizontal

2

Work out the joint width and depth first, since the width to depth ratio controls how much movement the seal can take

3

Allow for the backer rod, which sets the depth and stops the sealant bonding to the back of the joint

4

Check whether the substrate needs a primer, because most sealant failures are adhesion failures

5

Measure the total run in metres, as sealant is ordered by joint volume and not by floor area

Common Mistakes to Avoid

  • Filling a joint solid with no backer rod, which bonds three sides and tears the seal on the first movement
  • Making the joint too deep for its width
  • Skipping the primer on a porous substrate
  • Ordering by floor area rather than by metres of joint

What You Can Expect

Availability

Project order against a measured joint schedule

Coverage

UAE wide supply with GCC export support

Branch Support

Quotations and site coordination from Dubai, Abu Dhabi and Sharjah

Technical Guidance

Help working from joint width, depth and run to the pack count

Documentation

Weber data sheets for submittals, on each product page

Frequently Asked Questions

It comes from the joint, not the floor area. Multiply width by depth by the total run to get the volume, then divide by what the pack holds. Send us those three numbers and we will do it with you.

It sets the depth of the seal and stops the sealant sticking to the back of the joint. A sealant bonded on three sides cannot stretch and tears the first time the joint moves.

Gun grade holds its shape, so it is used on vertical and overhead joints. Pouring grade is self levelling and is used on horizontal joints in floors.

On most porous substrates yes. The sheet for each sealant says which primer and where. Adhesion failure is the usual reason a joint seal lets go, and it almost always traces back to preparation.

Working out a sealant quantity?

Send us the joint width, the depth and the total run in metres.

Share these details for a quick response:

  • Joint width and depth
  • Total run in metres
  • Vertical or horizontal, and the substrate